We are working on an assignment wherein stelliting 6 is required on Inconel pipe N 06625
The process used is GTAW, we are trying with below parameters but obeserving cracks on weld.
preheat: 275 deg C
Interpass: 300 deg C
cooling: wrapping in asbestos blanket.
Need an expert view to get the crack free weld .I tried contacting expert in this field locally, but they are not able to resolve the issue. they only adviced that low thermal gradient is required as material is hard.
Does any body has done similar welding successfully & can share their views.
The process used is GTAW, we are trying with below parameters but obeserving cracks on weld.
preheat: 275 deg C
Interpass: 300 deg C
cooling: wrapping in asbestos blanket.
Need an expert view to get the crack free weld .I tried contacting expert in this field locally, but they are not able to resolve the issue. they only adviced that low thermal gradient is required as material is hard.
Does any body has done similar welding successfully & can share their views.