Nov 12, 2014 #1 GadflyHu Materials Joined Sep 3, 2014 Messages 3 Location CA Hi @Steamdog, As you mentioned in thread408-255437, your working partner suggested that Stellite alloy should not be applied in Amine environment. Did he/she mentioned the failure situation or the reason. Thanks!
Hi @Steamdog, As you mentioned in thread408-255437, your working partner suggested that Stellite alloy should not be applied in Amine environment. Did he/she mentioned the failure situation or the reason. Thanks!
Nov 12, 2014 1 Thread starter #2 GadflyHu Materials Joined Sep 3, 2014 Messages 3 Location CA Thank you very much in advance for any information Upvote 0 Downvote
Nov 12, 2014 Thread starter #3 GadflyHu Materials Joined Sep 3, 2014 Messages 3 Location CA Anyone with information is welcomed. Thanks! Upvote 0 Downvote