Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Steel coupons sizes for mechanical testing of existing steel to a building structure

Status
Not open for further replies.

Ingenuity

Structural
Joined
May 17, 2001
Messages
2,374
Location
US
I have a project constructed with structural steel that is existing and without original structural drawings (more than 50 years old), so we do not know too much about the mechanical properties of the steel used.

We propose to take field coupon of selected members (mainly W sections) and have a lab conduct mechanical testing (yield, tensile, elongation etc.).

Based upon ASTM A370 the dimension of the required coupons are rather large: 8" x 2"

steel_coupons_ovfp7m.png


Does anyone have experience with sampling field coupons that are smaller than the above, or know if another ASTM (or AISC) document permits smaller coupon sizes?
 