Does anyone have a piping spec covering steam at 61 Barg (900psi) and 442 Deg C (827F) for ANSI B31.1. I'm looking for piping materials, standards, fittings, etc over a range of sizes.

Any help appreciated.


Regards,

Chris
 
Replies continue below

Recommended for you

I will not use carbon steel pipe for this high temperature service. At least C-0.5Mo steel (pipe ASTM A335-P1) should be used.
 