Nov 23, 2004 #1 Peckett Mechanical Joined May 6, 2002 Messages 29 Location NZ Does anyone have a piping spec covering steam at 61 Barg (900psi) and 442 Deg C (827F) for ANSI B31.1. I'm looking for piping materials, standards, fittings, etc over a range of sizes. Any help appreciated. Regards, Chris
Does anyone have a piping spec covering steam at 61 Barg (900psi) and 442 Deg C (827F) for ANSI B31.1. I'm looking for piping materials, standards, fittings, etc over a range of sizes. Any help appreciated. Regards, Chris
Nov 23, 2004 #2 PAN Mechanical Joined Apr 25, 2001 Messages 549 Location SG I will not use carbon steel pipe for this high temperature service. At least C-0.5Mo steel (pipe ASTM A335-P1) should be used. Upvote 0 Downvote