Could someone advise me on a typical pipe specification for a steam line 14 barg operating at 210°C(slightly superheated).
Thanks
 
ASTM A106 GR A

luismarques
 
Schedule 40 up to 10" with ANSI 300 fittings. That will give a 260 C and 40 bar rating.
 
sorry I forgot to say it is a 12" line.
 
amanites

Be sure and check with B31.3 (most commonly used for steam lines) or B31.1 when looking at your overall system components & design.

You may want to look at ASME SEC I, Figure 100.1.2, A & B (in B31.1)

There have been some good threads on steam lines/systems, a search will turn them up.

Greg Lamberson, BS, MBA
Consultant - Upstream Energy
Website:
 
12" sch 40 would be good for 35 barg
 