Jul 11, 2007 #1 amanites Mechanical Joined Mar 23, 2007 Messages 21 Location BE Could someone advise me on a typical pipe specification for a steam line 14 barg operating at 210°C(slightly superheated). Thanks
Could someone advise me on a typical pipe specification for a steam line 14 barg operating at 210°C(slightly superheated). Thanks
Jul 11, 2007 #2 0707 Petroleum Joined Jun 25, 2001 Messages 3,453 Location PT ASTM A106 GR A luismarques Upvote 0 Downvote
Jul 11, 2007 #3 dcasto Chemical Joined Jul 7, 2001 Messages 3,570 Location US Schedule 40 up to 10" with ANSI 300 fittings. That will give a 260 C and 40 bar rating. Upvote 0 Downvote
Jul 11, 2007 Thread starter #4 amanites Mechanical Joined Mar 23, 2007 Messages 21 Location BE sorry I forgot to say it is a 12" line. Upvote 0 Downvote
Jul 16, 2007 #5 GregLamberson Petroleum Joined Dec 2, 2006 Messages 577 Location US amanites Be sure and check with B31.3 (most commonly used for steam lines) or B31.1 when looking at your overall system components & design. You may want to look at ASME SEC I, Figure 100.1.2, A & B (in B31.1) There have been some good threads on steam lines/systems, a search will turn them up. Greg Lamberson, BS, MBA Consultant - Upstream Energy Website: http://www.oil-gas-consulting.com Upvote 0 Downvote
amanites Be sure and check with B31.3 (most commonly used for steam lines) or B31.1 when looking at your overall system components & design. You may want to look at ASME SEC I, Figure 100.1.2, A & B (in B31.1) There have been some good threads on steam lines/systems, a search will turn them up. Greg Lamberson, BS, MBA Consultant - Upstream Energy Website: http://www.oil-gas-consulting.com
Jul 17, 2007 #6 dcasto Chemical Joined Jul 7, 2001 Messages 3,570 Location US 12" sch 40 would be good for 35 barg Upvote 0 Downvote