I am trying to find something in an AWS spec that gives me more information about welding stainless to carbon steel. I know I need a 309 electrod but I need something in AWS to reference for the customer I have.
I looked in D1.6 and could not find stainless to carbon.
Any help would be great.
 
Replies continue below

Recommended for you

Look a little closer in D1.6. Toward the back, there are charts of suggested filler metals for different base metals. Carbon Steel is in there. Annex F, Table F.1
 
Thanks for the information. My current copy of the D1.6 is 1999. I have just ordered the current D1.6 and will look in in when it comes in. In my D1.6:99 Annex F is "Sample Welding Forms".
 