I am designing fillet welds for a moment connection of two HSS tubes made with 316 stainless. I want to use AISC Table 8-4 for the weld group but I am not familiar with weld strengths in stainless
and not sure what electrode to choose from Table 8-3 to arrive at the C1 coefficient. Can anyone who is up on stainless welding point me in the right direction?
Thanks for your help/advice.
 
AISC's Design Guide 27 would be a good place to start: Link

I like to debate structural engineering theory -- a lot. If I challenge you on something, know that I'm doing so because I respect your opinion enough to either change it or adopt it.
 
KootK
Thanks for the info but unfortunately I am not a member of AISC>
 
Google harder.

I like to debate structural engineering theory -- a lot. If I challenge you on something, know that I'm doing so because I respect your opinion enough to either change it or adopt it.
 
Some exerpts.

IMG_4837_khdnnx.png

IMG_4838_iee1or.png


I like to debate structural engineering theory -- a lot. If I challenge you on something, know that I'm doing so because I respect your opinion enough to either change it or adopt it.
 
$140/yr to join AISC and you can get all 29 Design Guides for free. Plus all of the other free info that is on there...best membership deal out there that I am aware of!
 
ASCE gives you several hours of free PDHs. It's not a bad deal if you like the free classes that are on the list for any given year.
 