Can you get headed studs in stainless? Are they designed like a normal headed stud? or can normal carbon steel headed studs be welded to stainless steel without problem?

In addition is there a fastener like Tapcon that is available in stainless steel?

Thanks, Dik
 



 
Thanks... I didn't know that Tapcons come in SS.

Can carbon steel headed studs be welded to SS plate? The movie shows it can be done. Thanks, again...

Is there a commercial product that can be used for passivating stainless steel weld. It's such a 'common' connection that there should be a commercial product.

The connection looks like this:
1749017982207.png
 
Last edited:
Thanks... I didn't know that Tapcons come in SS.

Can carbon steel headed studs be welded to SS plate? The movie shows it can be done. Thanks, again...

Is there a commercial product that can be used for passivating stainless steel weld. It's such a 'common' connection that there should be a commercial product.

The connection looks like this:
View attachment 10345
Dik, I've had contractors use this stuff before: https://www.derustit.com/products/wonder_gel.php

This was used for field welds. I don't know what is used in the shops on fabricated pieces, but our specifications require P&P on any welded element.

And yes from my understanding SST can be welded to carbon. Can't say I've done it. I usually try to find a way to avoid that. More from my lack of understanding than it really being an issue.
 
I would recommend Elco (now owned by Dewalt) Bi-Flex 300 series stainless steel screws - Ductile body with hardened tip, better for hydrogen corrosion embrittlement/HSCC
 
Last edited:
I think the SS Tapcons are 410 grade which still rusts pretty easily
 
I would recommend Elco (now owned by Dewalt) Bi-Flex 300 series stainless steel screws
Thanks... I'll look into them; I was planning on using Tapcons but these could be better. The client would not like rust.
 
What is the purpose of the screws? Just wondering if there isn’t a better method of attachment, the screws for concrete have a nasty habit of snapping when installing and the heads get beat up on install
 
What is the purpose of the screws?
There's another part of the project that requires them...
1749099175631.png
And yes from my understanding SST can be welded to carbon.
I was talking to a welder and they often use 306 wire; I have to check what this product is and what the actual spec for it is.
 
I wonder if you could use flush concrete insert anchors and a flush machine screw.
 
I wonder if you could use flush concrete insert anchors and a flush machine screw.
I haven't asked, but I suspect the architect doesn't want to see fasteners.
 
FWIW - The Biflex screws come in under-cut head (though the number of options is somewhat limited)
 
Simpson has a stainless steel anchor for that. Goes down to a minimum of 1/4"Ø.
1749138536386.png
 
Thanks for the info, gentlemen... I didn't realise there were so many available...
 
I just realized I gave you a metal to metal "Tek style" screw. But Dewalt does make the Agge-gator, which is similar to the Bi-flex, but for concrete / masonry. My apologies for the confusion.
 

Part and Inventory Search

Sponsor

Back
Top