For all those who cut stainless on a amada fo-3015 fanuc series 160i-L, do you use nitrogen, or oxygen?

If oxygen what lens, and nozzle do you use?
 
how thick are you cutting? Nitrogen is a must is you want any kind of edge quality.
 
I figured. I'm cutting 3/8 thick. I know that nitrogen is the right way to go, just wondered if anyone has done it with oxygen.
 