Martin_Arc
Petroleum
Hi All,
we have a pending order with an US Oil Major which contains of:
Seamless Pipes in A106 (thickness<19mm)
Plates in A516 gr70 (t>19mm)
Flanges in A105 and A350 LF2
Forged Nozzles in A105 and A350 LF2
The materials are needed for a pressure vessel.
After some weeks they come back to us asking for a simulated post weld heat treatment on all materials.
This sound strange to me. As far as I know ASME does not require a PWHT for such materials. So why a sWPHT.
My experience/feeling with steel in oil and gas tells me this request is invalid, but since I am not an engineer I cannot find correct literature to support this.
Or am I mistaken and is the sPWHT a valid request?
thanks,
Martin
we have a pending order with an US Oil Major which contains of:
Seamless Pipes in A106 (thickness<19mm)
Plates in A516 gr70 (t>19mm)
Flanges in A105 and A350 LF2
Forged Nozzles in A105 and A350 LF2
The materials are needed for a pressure vessel.
After some weeks they come back to us asking for a simulated post weld heat treatment on all materials.
This sound strange to me. As far as I know ASME does not require a PWHT for such materials. So why a sWPHT.
My experience/feeling with steel in oil and gas tells me this request is invalid, but since I am not an engineer I cannot find correct literature to support this.
Or am I mistaken and is the sPWHT a valid request?
thanks,
Martin