Jun 13, 2006 #1 johnbe Mechanical Joined Mar 23, 2005 Messages 1 Location US Is it possible to spheroidize 1144 alloy steel?
Jun 13, 2006 #2 swall Materials Joined Sep 30, 2003 Messages 2,767 Location US Yes, 1144 can be spheroidized. But, if you are hoping that this will increase some formabililty parameter, you may be out of luck, as the sulfur inclusions will then be the limiting factor for formability. Upvote 0 Downvote
Yes, 1144 can be spheroidized. But, if you are hoping that this will increase some formabililty parameter, you may be out of luck, as the sulfur inclusions will then be the limiting factor for formability.
Jun 13, 2006 #3 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US As swall said, 1144 steel can be spheroidize annealed. Upvote 0 Downvote