How are people specifying the use of recycled wood for structural purposes?
I have a situation where a contractor wants to reuse wood trusses which they have pulled down from elsewhere on the project in-lieu of framing which has been specified on construction documents.
Generally I request the builder to submit evidence that the wood which turns up onsite complies with the standard set-out in the specification and likewise for moisture content and preservation treatment. How would this be achieved if the wood is reused? What must be performed to ensure that this wood is up to standard?
I have a situation where a contractor wants to reuse wood trusses which they have pulled down from elsewhere on the project in-lieu of framing which has been specified on construction documents.
Generally I request the builder to submit evidence that the wood which turns up onsite complies with the standard set-out in the specification and likewise for moisture content and preservation treatment. How would this be achieved if the wood is reused? What must be performed to ensure that this wood is up to standard?