Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

specific heat of molten cast iron

Status
Not open for further replies.

brennan

Mechanical
Joined
Sep 4, 2002
Messages
1
Location
US
I am looking for the specific heat of molten (2750 F) cast iron.
 
The only info I could find on this subject is from ASM HANDBOOK Volume 1:

Heat of fusion for ferritic and pearlitic grades of ductile iron is about 210 to 230 kJ/kg (90 to 99 Btu/lb).
 
I assume you are looking for the heat capacity of liquid iron - a value I have from school work is 754 J kg-1 K-1.

The data TVP gave you, more correctly referred to as melting enthalpy, is for a different entity also needed for solidification analysis.
 