May 30, 2006 #1 pardissss Mechanical Joined Mar 17, 2006 Messages 17 Location IR Equivalent of St.37-3N?
May 30, 2006 #2 ijzer Materials Joined Oct 25, 2002 Messages 313 Location NL Is structural steel , normalized and impact tested at minus 20 Deg.C Upvote 0 Downvote
May 31, 2006 Thread starter #3 pardissss Mechanical Joined Mar 17, 2006 Messages 17 Location IR Thanks very much ,just wanted to know the equivalent of this material.name of material which could be replaced instead of St.37-3N yours, pardiss Upvote 0 Downvote
Thanks very much ,just wanted to know the equivalent of this material.name of material which could be replaced instead of St.37-3N yours, pardiss
May 31, 2006 #4 diamondjim Mechanical Joined Jul 30, 2000 Messages 992 Location US Try this: http://www.mesteel.com/info/equivalent.htm Upvote 0 Downvote