Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Sonic velocity of Si3N4 2

Status
Not open for further replies.

Cleopatra

Materials
Joined
Jan 5, 2003
Messages
10
Location
DE
Hi,

I am looking for sonic velocity of silicon nitride but I could not find it anyway.Can somebody help me?

Thanks,

 
Here is the data that I have. I have no information as to the specific material.

Silicon Nitride.

VL mm/micro s 11.06

VS mm/micro s 6.25

Density g/cm3 3.27

ZL Mrayl 36.0

 
The Coors data doesn't list sonic velocities, but

Hot pressed, density = 3.31 and modulus = 311GPa
reaction bonded, density = 2.5 and modulus = 179GPa

And I don't remember how to calculate it.

= = = = = = = = = = = = = = = = = = = =