We are trying to repair rust pits at water jackets on a cast iron block with Solder and so far are unsuccessful. We've tried rod, silver solder with flux, tried arc welding with low melting point nickel rod none of which worked. Is there a way to solder cast iron at low temperature, keep cast iron below 400F?