Dear All,

I wanted to find out if the speed my computer is working correctly for Sol 600 non linear solves. Right now i utilize a machine:

Windows 7 64bit
16 Gigs DDR
Intel Core I5 CPU 650@3.2Hz

I am running a TET10 model with 200K nodes with non linear aluminum (A356) material and basic loads. I load the model up over 1sec and unload it down for 1sec. My results are correct with stresses around 250 MPA and low strains under 3%.

However, each job is taking about 120-150 minutes depending on the number of cut backs. Ddes this solution time sound reasonable for this kind of model running on a 64 bit machine? I thought it would be faster.

I am curious about solve times for a 200K node model running on other machines. Any thoughts, maybe a setting,parameter or configuration I am missing?

Thanks ahead of time.
 
I won't be able to really help you, but not that one of the most important specs for calculation speed is your graphics card. So you should probably mention that one as well.

NX 7.5.5.4 with Teamcenter 8 on win7 64
Intel Xeon @3.2GHz
8GB RAM
Nvidia Quadro 2000
 