Has anyone used chainlink fence as reinforcement for shotcrete slope paving? I have a client who wants to use the chainlink as an alternative to WWF for slope paving for permanent erosion control. The ground surface is fairly irregular making the chainlink much easier to install. The chainlink will be supported on rebar and then shotcrete will be applied over the top. Becuase it's essentially a non-structural application, I can't think of a good reason to say no. Additionally, the chainlink is galvanized and the reinforcement ration is higher. Any feedback would be greatly appreciated.
Thanks.
Thanks.