TangoCleveland
Mechanical
We are welding a 48" 150RF B16.47 slipon flange to a 3/8" wall pipe. For fitup adjustment, B31.3 gives minimum depth equal to pipe wall thickness for the internal weld. What's the maximum we can move the flange out? I found nothing in B31.3 for the maximum. ASME Sec VIII Div 1 and 2 show the maximum is pipe wall plus 1/4"; we need pipe wall plus 5/8". Our boilermakers say that their practice is to use 1/2 the thickness of the flange as a maximum (dimension "C" in B16.47).
In general, what's the maximum permissible projection of a slipon flange off the end of the pipe?
Larry
In general, what's the maximum permissible projection of a slipon flange off the end of the pipe?
Larry