Hello All,
According to B31.1, Table A-3, General Note (1) allowable stress values tabulated for temperatures over 1,000°F apply only if the carbon content of the material is 0.04% or higher.
Is this note also applicable for welding material?
Can I use ER316L for welding SA312-TP316 for temperature over 1000°F?
Thanks,
According to B31.1, Table A-3, General Note (1) allowable stress values tabulated for temperatures over 1,000°F apply only if the carbon content of the material is 0.04% or higher.
Is this note also applicable for welding material?
Can I use ER316L for welding SA312-TP316 for temperature over 1000°F?
Thanks,