shyamshins
Mechanical
Dear sir,
I need solution for single dry seal for agitator which failed at one of our site during operation.
Rotary carbon has came out of anti rotation pin, carbon got stuck to silicon carbide stationary face and drive pins rubbed on outer diameter of carbon removing its material.
I guess this is slipstick but unable to understand how I can solve this problem for which I need forum members help.
Process details are as follow:
PRODUCT: Cetirizine Dihydrochloride
OPERATING TEMP. 100 DEG.CELCIUS
RPM: 58
SP.GR.: 0.87
OPERATING PRESS.: Atmospheric and Under vacuum
About 20 % solid ( fine powder form ) added in Solvent,after addition of solids free flowing reaction mass available inside the reactor.
This is a dry seal and no lubrication is provided.
I am attaching photos of failed seal as well as of seal drawing.
Need your help to resolve this problem.
I need solution for single dry seal for agitator which failed at one of our site during operation.
Rotary carbon has came out of anti rotation pin, carbon got stuck to silicon carbide stationary face and drive pins rubbed on outer diameter of carbon removing its material.
I guess this is slipstick but unable to understand how I can solve this problem for which I need forum members help.
Process details are as follow:
PRODUCT: Cetirizine Dihydrochloride
OPERATING TEMP. 100 DEG.CELCIUS
RPM: 58
SP.GR.: 0.87
OPERATING PRESS.: Atmospheric and Under vacuum
About 20 % solid ( fine powder form ) added in Solvent,after addition of solids free flowing reaction mass available inside the reactor.
This is a dry seal and no lubrication is provided.
I am attaching photos of failed seal as well as of seal drawing.
Need your help to resolve this problem.