Does anyone have a handle on an injectable grade silicone rubber that will stick to a polycarbonate alloy substrate (insert molded)? Wanted in black...

Thanks
craig
 
Replies continue below

Recommended for you

Interesting stuff. Thanks for the tip.
 
Try Wacker Silicones. They have some new grades two component Platinum catalyzed silicone rubber for injection molding on the market specially made for overmolding different thermoplastics.
 