Only the people that have to have front surface mirrors. Front surface mirrors are used a lot with I.R. devices.
It was mentioned to me on time that a company was trying to produce a highly polished SiC thin disc which was giving them a lot of trouble. There was no mentioned of an end use and I didn't ask as this company did a lot "black project work".