I'm struggling to determine the force to reduce this sheetmetal spring to Ø17.8mm.

If someone could point me in the direction or give advice, that would be great. I can find alot about normal wire springs, but can't find much for a sheetmetal spring. The spring is 0.6mm thick and 10mm long.

Thanks!Sheetmetal Spring.jpg
 
Op
How many, quantity?
Low volume 10 pcs, or 10000 parts.
This is a great brain teaser.
My thoughts and opinion.
Thus a very small part. I would first of make a new design.
OK but if you are set on this.
It will require developing.
Trial and error to allow for spring back.
A two or three stage die. Reason the leg
Pushed into the center.
Create the two small bends on b each end.
Then the large radii
Then bend the inner leg.
Depending on hardness, or tensile strength.
For small lot a small fixture with removable pins. Similar use for bending tubing.
HTH
 
Out of curiosity, I revisited the original method and updated it to be in-line with the polar method (same assumed forced radial displacement, point loading at start of contact not in middle of angular increment, etc). The result gives a bending stress of 196.7 MPa. Although it hasn't been checked, and as rothers has highlighted, the stress is close to FEA. Attached is the revisited file. Looks like this particular analytical method has been finalized!
 

Attachments

My FEA is not great at post processing contact forces but for what it's worth here goes:

Reaction force contour plot:
Interestingly reactions concentrated in three places, sum of reactions are:
Left hand contact point = 15.37 N
Bottom contact point = 15.37 N
Right hand contact point = 14.33 N

spring_reaction.png

Reaction Force Vector plot:
Ignore the exact position of the vector, it plots the vector start points at the final contact point of part 1 (the ring) but at the initial contact point of part 2 (the spring).
Anyway I'm sure you get the idea and is shows the directions nicely.
spring_reaction_vector.png

Make of this what you like !!
 
Just thought I'd post this last adjusted calculation. By altering the forced displacement, the polar method now calculates a maximum bending stress of 212.3 MPa and an initial contact load of 14.47 N. This compares well to the posted FEA results. Attached is the adjusted file.
 

Attachments

maybe something like a jubilee clip ... to compress the OD ?

or a tool to pick up the two obvious hooks, and shorten the distance between them ? Option 1 sounds easier ....
 
Just to simplify things, here's a two pager showing the results for a single point load at the free end, based on an assumed forced displacement and at varying contact angles.
 

Attachments

Last edited:
This problem should be solved by a simple analysis.
Assume the force needed to compress the spring is appllied by a circlip plier between the two hooks. This force F has a vertical component V=~0.93F and an horizontal component H=~0.36F (estimated from geometry).
Now assume also, for simplicity, that F acts onto the outer hook, while the inner hook is connected to a pin.
The bending moment in the spring due to V is -Vr sin(theta) (theta from 0 to 1.5pi), and the moment due to H is Hr(1-cos(theta))
So the average bending moment in the spring is Mave=Fr*integral(0.36*(1-cos(theta))-0.93*sin(theta))/1.5pi=~-0.24Fr
From the relationship (delta r)/r2=-Mave/EI, with delta r=0.2 mm, one obtains F=46 N
This seems a relatively high value, so please correct me if I'm mistaken
 