Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Shaft Step Stress Concentration

Status
Not open for further replies.

DAVIDSTECKER

Mechanical
Mar 23, 2005
526
I am working on the design of an output shaft for a gearbox and need some input about a type of fillet for the step between two different diameters.
I know the general rule is to use as large of fillet as practical, but some time ago I ran across a design that actually plunged into the smaller diameter then went straight up the face to the larger diameter.
This was supposed to be better than just a fillet in the 90 deg. step.
Does anyone have experience with this practice and is it the better way to go?
Best regards, David
 
Replies continue below

Recommended for you

Cool web site, thanks.
The under cut I saw came in at a slight angle as it approached the step, and then left the radius. Not quite a "full" groove.
Actually this design was shown to me by someone at a major electric motor company and he said that this practice all but eliminated failures.
 
I did a search and came up this thread that sounds some what like the relief I'm talking about.
thread2-106261.
What do you think?
 
David,

The stress concentration will be at a minimum when using a large radius. The groove feature that you mentioned is better than a sharp corner, but not as good as a large radius. It is used when a radius cannot be accommodated, due to a bearing sitting on the face of the larger diameter portion, etc.
 


Gearboxes and PTO's often use these to define a break point if there is gong to be one.

Step downs are also used at the end of splines. The jury is still out as to whether a step down is better or worse than spline groove ends.



 