Mechatronic,
There are a number things to consider when selecting a mechanical seal for an API 610 application;
Liquid Pumped
Temperature (very important)
Solids ( per cent)
Is the liquid agressive
Type of Pump being used
Is there a vacuum
Discharge and suction pressures
location of pump
Speed
All of this can be overwhelming but it's really not hard once you get into it.
If it agressive- use a material that will be compatable
If you need a pipe plan for dirty pumpage you can choose from;
PLAN 31; recirulation from pump case thru a cyclone separator delivering a clean fluid thru a cooler to the seals and putting the solids back into the pump suction
PLAN 32; injection to seal from external source of clean fluid.
PLAN 33; circulation of clean fluid to a double seal from an external circulation system.
You also have Plan"A" thru Plan"L" for cooling water piping and others as well, using throttle bushings, external seal reserviors, dead ended blankets ( for methanol, external fluid quench and barrier fluids.
You have some good seal people out there but be aware they there to sell you their product and it could be costly if your not careful. All API 610 Applications use an API 682 mechanicl seal.
Regards,
Jimbo986