How do we get thicknesses and materials for wps/pqr in a piping project? Is it from drawings or any other documents?

There could be thousands of drawings in a project
 
Replies continue below

Recommended for you

Steve_mechanical,

Are you designing or manufacturing? If you are designing, you determine all that based on your requirements. If you are manufacturing, your customer hands you drawings and/or a contract.

--
JHG
 
There needs to be a master list of all welds, alloys, p No, thickness, weld type, psoition.
The you can build the list of procedures and make sure that they are all covered.
And then you can sort out how many different qualifications will be required.
I start with the BoM and make sure that those are all adressed.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Ed is giving the right direction. Start with the bill of materials to determine what you will be welding.
In general, the thickness qualified will be 1/2T to 2T where T is the thickness of the test coupon used to qualify the WPS. Now, 1/2T to 2T is a white lie, but it is a starting point. You didn't provide us with information regarding the governing welding code. You mention pipe, so perhaps ASME applies. That being the case, Section IX would provide more specific information. Depending on the thickness you use, the thickness range could be 1/16-inch to 2T or if the test piece is thicker or equal to 1 1/2-inch the thickness range could be 3/16-inch to 8-inches.