Dear All

Good day.


I wanted some expertise on the basis of selection of duplex and CRA materials.

I have seen duplex, super duplex, 6Mo ( UNS 31254), inconel ( UNS 6625), incoly ( UNS 8825), Clading by 6625 / 8825 in piping material class for process hydrocarbon / well head fluids.

How we can select the suitable one from the above if we have a system. Is this based on MSR report?

Pls share your experience
 
Replies continue below

Recommended for you

Choice is based on the severity of the service conditions, and 'other folks' experience with those conditions and fluids. Hopefully, your fluid and conditions [temp. & pressure, flow velocity] are documented in the reference literature -- then use the recommended stuff.

With undocumented conditions and fluid, start doing corrosion rate studies to include highly stressed coupons that get tested for Stress Corr. Cracking. Good Luck - it takes a couple of years and a bunch of lab time. And you may have the same result we had; no metals [other than tantalum and possibly gold] would work. We went to glass-lined and still 'use up' a reactor in less than 1-year.
 
Metallurgy selection is based on fluid(s) temperature, pressure, % water, % H2S, % CO2, % Chlorides, etc. both now and expected in the furure. It's also determined by overall economics over the life of the well and whether or not to use corrosion inhibitors. I suggest you employ the talents of a corrosion metallurgist experienced in the field.
 