cvg
Civil/Environmental
- Dec 16, 1999
- 6,868
I'm trying to specify stainless steel bars (3/4" or 1" diameter, hex or square x 18" long) to be used in an abrasive environment as a survey monument. They will need to be welded and very hard to resist erosion. I'm looking at cost, availability and workability. Specifically 303, 304 and 316. Which would be the best?