jakinsjh
Mechanical
- Aug 15, 2013
- 3
Anybody please correct my seal selection for following :
Service : Centrifugal Feed Pump
Liquid : Hot lime softener sludge slurry
Seal & Plan : Single mechanical seal + Seal plan 23 ()
Liquid properties ----------------------------------------
TDS = 933 mg/l Total Hardness(as CaCO3) = 25 mg/l
TSS = 53000 mg/l P ALK = 179 mg/l
TOC = 383 mg/l M ALK = 348 mg/l
Silica (as SiO2) = 50 mg/l
Chlorides 278 / 4000 mg/l
Oil = NILL
pH = 10.2
-----------------------------------------------------------
Service : Centrifugal Feed Pump
Liquid : Hot lime softener sludge slurry
Seal & Plan : Single mechanical seal + Seal plan 23 ()
Liquid properties ----------------------------------------
TDS = 933 mg/l Total Hardness(as CaCO3) = 25 mg/l
TSS = 53000 mg/l P ALK = 179 mg/l
TOC = 383 mg/l M ALK = 348 mg/l
Silica (as SiO2) = 50 mg/l
Chlorides 278 / 4000 mg/l
Oil = NILL
pH = 10.2
-----------------------------------------------------------