Screening Tools for Piping Systems

Status
Not open for further replies.

James01

Petroleum
Joined
Feb 4, 2003
Messages
38
Location
GB
I have a closed drains system on my platform that is fully welded from start to finnish of diameters varying from 2" up to 10" diameter. There is approximately 5 miles of pipework in the system. It has multiple elbows and branches and has been in service for 23 years.

I know that there are SRB's in the pipework and need to screen the system to target inspection.

Does anyone know of a quick and reliable method?
 

What comes to mind:

1. Portions of the closed drain system upto 4";
RT-DWDI; you can readily identify corrosion
across the pipeline wall.

2. Thickness and or flaw detection survey.

2.1 Guided Wave-UT to cover considerable pipeline
lenght. (assess material loss)

3. Hydrostatic Testing.

4. Assuming portions of the pipping is U/G ; DCVG/CIPS
to survey the coating system.

5. Pipeline profile (Low/High Points) prone to fluid
accumlation or stagnant conditions.

The above can be utlized to a level of coverage that would
provide assurance; in combination of or all.

Cheers



 
PVRV

Thanks for the info. We have already done random UT & Radiography and found problems. I am looking at GUL & LORUS at present but have lots of branches & elbows to contend with.

SLOFEC is another option?

Cheers
Jim
 