MrTungsten
Materials
Hi Expert,
I have some question regarding Flux Type of SAW with 625 filler metal ,
Is there anybody here which have some experience about SAW with 625 filler metal ? Is there any concern about solidification crack with the flux of SAW 625 or there is another concern ? is there any brand which recommend for SAW flux and filler ?
we want to perform SAW to increase high productivity of 625 filler butt weld.
Your advise will be valuable
Thanks and Regard's
I have some question regarding Flux Type of SAW with 625 filler metal ,
Is there anybody here which have some experience about SAW with 625 filler metal ? Is there any concern about solidification crack with the flux of SAW 625 or there is another concern ? is there any brand which recommend for SAW flux and filler ?
we want to perform SAW to increase high productivity of 625 filler butt weld.
Your advise will be valuable
Thanks and Regard's