Hello,
I am getting the welds in a tube examined by NDE (ultrasonics). I need to prepare the welds on the inside of the tube (which is a confined space).
The thickness of the tube is extremely important. The NDT technician has requested sand blasting, I do not want to remove any material from the tube.
I am aware of different types of sandblasting media - walnut, CO2, different sized garnet.
I am very reluctant to use C02 given the confined space and the associated atmospheric changes. Does any one have any information on the surface removal depth of ordinary garnet or walnut shell?
Thanks.
I am getting the welds in a tube examined by NDE (ultrasonics). I need to prepare the welds on the inside of the tube (which is a confined space).
The thickness of the tube is extremely important. The NDT technician has requested sand blasting, I do not want to remove any material from the tube.
I am aware of different types of sandblasting media - walnut, CO2, different sized garnet.
I am very reluctant to use C02 given the confined space and the associated atmospheric changes. Does any one have any information on the surface removal depth of ordinary garnet or walnut shell?
Thanks.