powerplantcwi
Mechanical
My company is being asked by a client to weld SA213-T23 to a SA213-T12 boiler wall tubes, using a temperbead welding procedure to eliminate any carbon migration issues caused by PWHT. In all the research I've read, I can find no recent information supporting any welding T23 material without PWHT. As it is currently unassigned in ASME Section IX, and therefore not addressed in the applicable ASME Sec I, I am just looking for a little advise with this relatively new material. We have a WPS utilizing ER90S-B3 and no PWHT that was developed in 2009, but in light of new research we will be using Bohler P23-IG or equivalent filler with PWHT for our new WPS's. Is thickness a determining factor for PWHT on this material?
Also I am in search of material to qualify the new WPS and am having trouble locating any of the T23, any leads would be appreciated.
Also I am in search of material to qualify the new WPS and am having trouble locating any of the T23, any leads would be appreciated.