ChiangJaron
Industrial
Deae Expert,
Background
Material SA-537 CL2
The product plate shall be delivery in heat treatment condition in Quenched and tempered.
And the tempering temperature is request 595℃ minimum as code.
Welding progress is SMAW with ASME SFA-5.5 E8016-G
PWHT and Impact test are required.
Questions:
1. Are there any specification/rule to limit tempering temperature in maximum temperature? and holding time?
2. Are there any recommendation for PWHT temperature shall lower than material tempering temperature?
3. Are there any recommendation for simulation testing of plate/electrodes shall consider PWHT failed risk to increase simulation holding time to 2 times?
Background
Material SA-537 CL2
The product plate shall be delivery in heat treatment condition in Quenched and tempered.
And the tempering temperature is request 595℃ minimum as code.
Welding progress is SMAW with ASME SFA-5.5 E8016-G
PWHT and Impact test are required.
Questions:
1. Are there any specification/rule to limit tempering temperature in maximum temperature? and holding time?
2. Are there any recommendation for PWHT temperature shall lower than material tempering temperature?
3. Are there any recommendation for simulation testing of plate/electrodes shall consider PWHT failed risk to increase simulation holding time to 2 times?