Hi All,

If somebody have stress values for SA-516 Gr.70 from ASME 1995 edition, I really appreciate it. I believe it was safety factor 4.0 at a time.

Thank you,

Curtis
 
Replies continue below

Recommended for you

17500 up to 650 F, over that, don't recall.
 
Which Section of ASME and which Division of the 1995 Edition are you specifically interested in? Any specific temperature?
 
TGS4, thank you, I should have added for Sec VIII, Div 1.
 