Apr 21, 2009 #1 luke7203 Chemical Joined Nov 22, 2004 Messages 5 Location US What are the advantages of an SA-350-LF2 tubesheet over SA-516-70? Thanks for the help!
Apr 21, 2009 #2 pastyl Mechanical Joined Feb 7, 2009 Messages 37 Location GR SA-350-LF2 material is appropriate for lower temperatures (up to -48Celsius) were SA-516-Gr70 possibly must be normalized and impact tested, according tubesheet thickness and design temperature (see UCS-66) Upvote 0 Downvote
SA-350-LF2 material is appropriate for lower temperatures (up to -48Celsius) were SA-516-Gr70 possibly must be normalized and impact tested, according tubesheet thickness and design temperature (see UCS-66)