In ASME II, Part D, Subpart 1 in table 3 the SA-325 Gr 1 structural bolt is classified for ASME III application NP=not permitted for maximum temperature limit, why is this bolt not allowed? The most curious thing is that the same table shows the SA-325 material without any classification and this material is applicable in ASME III.


2_hwrvfv.jpg
1_giqqqu.jpg
 
Replies continue below

Recommended for you

Other BPV sections do allow this material for code applications which is why it’s listed.

Huub
- You never get what you expect, you only get what you inspect.
 
DO NOT DUPLICATE THE PUBLICATION.

Regards
 
I don't understand the point of Line 3 with no Grade, UNS, or Diameter specified but I've never seen A-325 stud bolts used with pressure vessel flanges before. They are permitted in ASME Section VIII but I've only seen them used for anchor bolts or structural steel.


-Christine
 
Christine, I wondered about that as well, My old (2009) SA-325 lists bolts of Type 1 and Type 3 (weathering steel) only. No "untyped" bolts. I wonder if this was added in a newer Edition?

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
@ Maritza Ulloa
Is it a curiosity or do you really want the SA-325 for nuclear service?