Does anyone have the S-N Curve for 17-4 PH SST heat treated to H900? I want to use it in SolidWorks 2014 now that I can do fatigue analysis.
 
Replies continue below

Recommended for you

They are in the old Armco 17-4PH handbook.
My scans are selective and don't include the fatigue data.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 