May 19, 2014 #1 Dougt115 Mechanical Joined Oct 2, 2013 Messages 197 Location US Does anyone have the S-N Curve for 17-4 PH SST heat treated to H900? I want to use it in SolidWorks 2014 now that I can do fatigue analysis.
Does anyone have the S-N Curve for 17-4 PH SST heat treated to H900? I want to use it in SolidWorks 2014 now that I can do fatigue analysis.
May 19, 2014 #2 EdStainless Materials Joined May 20, 2004 Messages 16,385 Location Waukesha WI USA They are in the old Armco 17-4PH handbook. My scans are selective and don't include the fatigue data. = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote
They are in the old Armco 17-4PH handbook. My scans are selective and don't include the fatigue data. = = = = = = = = = = = = = = = = = = = = Plymouth Tube
May 19, 2014 2 #3 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Try here http://www.dtic.mil/dtic/tr/fulltext/u2/691794.pdf Upvote 0 Downvote
May 20, 2014 #4 tbuelna Aerospace Joined Aug 10, 2002 Messages 4,026 Location US Attached are S-N curves for 17-4PH H900 bar. These are curves for AMS 5643 material, which I believe is vacuum melt quality. So the data would not be accurate for air melt quality material. Hope that helps. Terry http://files.engineering.com/getfile.aspx?folder=9bbf8f25-8841-49dc-bbaa-2e4f4831be24&file=17-4PH_H900_S_N_curves.pdf Upvote 0 Downvote
Attached are S-N curves for 17-4PH H900 bar. These are curves for AMS 5643 material, which I believe is vacuum melt quality. So the data would not be accurate for air melt quality material. Hope that helps. Terry