Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

S-N curve for 17-4PH H900 2

Status
Not open for further replies.

Dougt115

Mechanical
Joined
Oct 2, 2013
Messages
197
Location
US
Does anyone have the S-N Curve for 17-4 PH SST heat treated to H900? I want to use it in SolidWorks 2014 now that I can do fatigue analysis.
 
They are in the old Armco 17-4PH handbook.
My scans are selective and don't include the fatigue data.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Attached are S-N curves for 17-4PH H900 bar. These are curves for AMS 5643 material, which I believe is vacuum melt quality. So the data would not be accurate for air melt quality material.

Hope that helps.
Terry

 
 http://files.engineering.com/getfile.aspx?folder=9bbf8f25-8841-49dc-bbaa-2e4f4831be24&file=17-4PH_H900_S_N_curves.pdf