I am designing S-beam for monorail, grade A36.
Can I find S-beam grade A992?
 
Per AISC Steel Construction Manual 14th Ed, Table 2-4: A36 is preferred material specification for S shapes. ASTM A992 material specification does apply to S shapes, however, the availability should be confirmed prior to specification.
 