Hello everyone,

I"m looking for an non-distructive device to measure moisture content in rubber rollers,some suggestions ?

Thanks!
Mihail
 
Replies continue below

Recommended for you

Why do you need to measure moisture content in rubber rolls? Are they foam rubber or solid rubber-based?
 

Sir,

I work at company which deals with remanufacturing cartridges for laser print, these have in structure a rubber rollers ( solid rubber) ; I want to know to what extent the moisture affects the performance of printing and now I´m trying to find a chemical solution to cover the rolls which have superficial defects like : pricks and/or scratches.
in my opinion, theoretical it is impossible because the rubber is vulcanized,
practical ....... we will see ?

Best regards,
Mihail.
 