Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

RT interpreter qualification

Status
Not open for further replies.

hdpinsp

Petroleum
Nov 11, 2013
5
If RT is for a B31.3 project what qualifications will be necessary for the personnel reviewing film.
 
Replies continue below

Recommended for you

While the Code only references SNT-TC-1A "may be used as a guide" under 342.1, Note 1, the Inspector has ultimate responsibility for accepting the certifications mandated to be provided by the Employer.
 
What weldstan said. What you are typically looking for is a Level II or III certification from that NDT lab. [VERY unusual to see a L/III out in the field. L/III's certify L/I's and L/II's]

If you are the Inspector, watch out for poor quality film - can't see the required IQI Image Quality Indicator; watch out for 'over-calls' on porosity. At 1/4" wall thickness, B31.3 allows 1.5 x as much porosity as on the Sect VIII porosity chart. Waaay too common for the L/II to reject a perfectly acceptable weld, because he/she saw "a lot of porosity". Use the charts - it is simple.
 
hdpinsp,
On a number of occasions while working for Engineering/Construction Management companies, I was appointed the Inspector by the Owner and had final authority regarding film interpretation (in some cases the only reviewer) and I did not have Level II or III certification in RT at the time.

As a contractor installing B31.3 pipe systems, we require RT to be performed by Level II or Level III certified examiners.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor