Roll bond clad is better than explosion bond, but is there any inspection/examination difference between them? Is roll bond more expensive than explosion bond?

Thanks.
 
Replies continue below

Recommended for you

Roll bond clad is better than explosion bond, but is there any inspection/examination difference between them?

Are you sure? Better check your sources.
 
that's what I was gonna say, but I considered it "opinion" and not fact....so I didn't

we use explosion bonded
 
lilili, I thnk I addressed this before on some other thread, but the decision to use roll- or expl- bonded clad can have more to do with cost and delivery than which is "better".

It seems Purchasing at my old company said you need to buy at least two pieces of roll bond because they roll them face-to-face. For one piece its det-bond or WOl.

Det bond may not be suitable for thinner backer metals, I'm not sure.

As always, "It depends."

Regards,

Mike

 