Hello everyone,
I have a Rerated and Altered pressure vessel (i.e. MAWP increased and replacement of reinforcement pads in nozzles were done). The Rerating point of API 510 (8.2.1 (d)) says that the pressure test could be avoid if "the vessel integrity is confirmed by special nondestructive evaluation inspection techniques in lieu of testing". BUT, that is for those equipment Rerated without any Alterations needed, so I think that in this case the vessel should be hydrostatic tested.
Someone thinks that in my case I could avoid the Hydrostatic Test?
Many thanks.
I have a Rerated and Altered pressure vessel (i.e. MAWP increased and replacement of reinforcement pads in nozzles were done). The Rerating point of API 510 (8.2.1 (d)) says that the pressure test could be avoid if "the vessel integrity is confirmed by special nondestructive evaluation inspection techniques in lieu of testing". BUT, that is for those equipment Rerated without any Alterations needed, so I think that in this case the vessel should be hydrostatic tested.
Someone thinks that in my case I could avoid the Hydrostatic Test?
Many thanks.