I have three questions:
1- The Epoxy coaltar Paint in my company is expired(according to paint manufacturer data sheet), but I decide to use it again and
claim that is usable.what is the complete tests for re qualfication of expired paints. considering that this paint is used for internal of firewater storage tank.
2-my paint engineer said that swelling test that used for evaluation of attack of tank fluid to paint, shall be employed.what is the swelling test for paints? and this test is required for re qualified of this Paint? for more information one paper about swelling of paint films is attached.
3- what is the detail procedure for adhesion test of Epoxy coaltar Paints According to SSPC-Paint16?
1- The Epoxy coaltar Paint in my company is expired(according to paint manufacturer data sheet), but I decide to use it again and
claim that is usable.what is the complete tests for re qualfication of expired paints. considering that this paint is used for internal of firewater storage tank.
2-my paint engineer said that swelling test that used for evaluation of attack of tank fluid to paint, shall be employed.what is the swelling test for paints? and this test is required for re qualified of this Paint? for more information one paper about swelling of paint films is attached.
3- what is the detail procedure for adhesion test of Epoxy coaltar Paints According to SSPC-Paint16?