I just returned from a church where the main roof beams are constructed using glulam and there is some serious delamination. I've provided them with 'emergency' information about shoring the existing structure; existing condition is dangerous. Glulam has 'gapped' approx 1/2" in places and split follows the tapered splicing of the 2x members.
I suspect the delamination has occurred because of high humidity and possibly a non waterproof adhesive. I'm in the process of trying to obtain construction documents.
Any suggestions about repairing delaminations? reconstruction may be an issue and repair costs could be several hundred thousand dollars.
Dik